Draft angle should not be a single number handed to every wall. A bare wall needs 0.5-1 degree. A textured wall needs the texture allowance added, conventionally one degree for every 0.025mm of texture depth. Deep cavities and thin walls need 2-3 degrees. When the angle is short, the side wall is dragged during ejection and shows as two white marks or a patch of cloudy scratches. Polishing fixes one batch; the next batch has them again.
The physics is simple. Plastic shrinks onto the core as it cools, and ejection has to overcome that grip. Draft converts part of that grip from friction into sliding, so a larger angle needs less ejection force. On a shallow cavity one degree is imperceptible. On a deep one it is obvious: on a 40mm deep wall, one degree and two degrees differ by 0.7mm of travel, and the ejection force can differ by a factor of two. When the force is insufficient the part is pushed white or punched through; when the force is raised to compensate, the wall starts to score.
Texture is where the number goes wrong most often. Texture is a field of microscopic pits in the tool, and the melt has to fill them. The deeper the texture, the harder the fill, and on ejection the plastic at the bottom of each pit is gripped by the tool, so every pit adds friction. The industry rule is one degree per 0.025mm of depth. A 20 micron texture adds 0.8 degrees on top of the one degree a bare wall would get anyway, so the drawing should read 1.8-2 degrees. What usually happens is that the drawing reads one degree, because the template says one degree and nobody changes it.
Fine texture at 10-15 microns needs 1-1.5 degrees. Medium texture at 20-25 microns needs 1.8-2 and is the most commonly under-specified band. Coarse texture and leather grain at 30 microns and above need 2.5-3, and the texture bottom has to be checked for fill. Deep cavities over 30mm need 2-3 on their own, added on top of any texture allowance rather than replacing it.
Deep cavities need more because the grip accumulates along the depth. On a deep tubular part with a 45mm wall, two degrees still produced slight scoring and 2.5 was stable. Thin walls are limited from the other side: below 1.2mm wall thickness, a large draft thins the wall at the base and hurts both strength and flow. The answer there is to reduce depth or change the parting, not to keep adding angle.
Direction matters as much as magnitude. Outer walls taper smaller toward the top and inner holes taper larger, both toward the ejection direction. Reversed, the part either will not release or the bore is torn on the way out. Two-shot and overmoulded parts need draft on the second cavity as well, and the deformation of the first shot has to be taken into account; these are the parts where draft problems surface only at trial, because the drawing review tends to skip them.
If a wall is already white, the repair depends on depth. Light surface whitening can be polished back. A visible groove can only be painted or scrapped. Before repairing anything, confirm whether the cause is insufficient draft or unbalanced ejection, because polishing will not save the next batch if the angle is the problem. Draft is set by the surface and the depth, not by the template.