When a screen print shows white along an edge, the first instinct is to replace the mesh. In most of the cases we have handled, the fault sits earlier: the registration datum is wrong. Three variables decide the result, in order of influence - the datum the print is aligned to, the squeegee angle, and the mesh tension.
A datum taken from the part's outer contour is unstable by construction. The moulding shrinks by about 0.1mm from part to part, and a slight flash on the edge moves the outline. That is why 0.2mm of drift is enough to open a white gap. Structural features are a different class: locating posts, ribs and snap slots are cut from the same steel and repeat within a much tighter band. Moving the datum from the outline to those features cut our per-part registration error from 0.10-0.26mm to 0.04-0.08mm. The change costs a fixture, not a new screen: two posts that seat on the part's own posts, plus a flat clamp.
Curved parts are a separate problem. The screen is flat and the part is curved, so contact starts at one edge, squeegee pressure varies along the stroke, and the edge either blurs or misses. A conforming fixture that holds the part parallel to the screen fixes it. On a curved panel we added a silicone pad as a compliant layer; as the screen came down the pad deformed and flattened the curve, and show-through fell from about thirty percent to single digits. That fixture usually costs less than remaking the screen, yet projects often skip it and blame the ink.
First-article inspection has three items: registration error, edge sharpness, and adhesion. The first two can be judged with eyes and a caliper; the third needs a cross-hatch test, and it has to wait. Ink adhesion is still climbing before full cure, so we require 24 hours after curing before the tape pull. More than five percent of the area lifting fails the part. Check the surface treatment first, then the bake temperature and time.
Process choice follows the same logic of matching the tool to the surface. If the longest edge of the graphic exceeds 30mm and the surface is close to flat, screen printing wins on speed and ink deposit. Small, scattered graphics on curved or irregular parts go to pad printing, which transfers through a silicone head. Either way the datum comes first: multi-colour work stacks registration error with every pass, so the more colours, the earlier the datum has to be fixed.
Texture is the other trap. A textured surface eats ink, breaks fine strokes, and above roughly 20 microns of etch depth fine lines simply will not print. If the mark must sit on texture, cut the texture shallower or polish it flat in that area - on the tool, which means deciding the print area and the texture zoning at the appearance review, not after the tool is cut.
Mesh tension, squeegee angle and screen gap set the ceiling once the datum is right. Standard tension is 18-22 N/cm; below 16 N/cm the mesh lags on release, the edge blurs. Squeegee angle runs 60-75 degrees: a shallow angle lays down more ink, a steep one less. Screen gap of 2-3mm balances sticking against edge spread.